Processing Guide:
|
PVC-C - Polyvinylchloride chlorinated
|
 |
|
Extruder:
|
Twin screw extruder with vacuum, plain feeding section
|
 |
|
Screw Design:
|
Four stage PVC screw (low-shear screw) three start precompression section 25 - 30 L/D
|
 |
|
Compression Ratio:
|
1,7:1
|
 |
|
Cylinder Temperatures:
|
180-195 C 356-383 F
|
 |
|
Melt Temperature:
|
180-195 C 356-383 F
|
 |
|
Pre-Drying:
|
no
|
 |
|
Calibration:
|
|
 |
|
Miscellaneous:
|
more sensitive to heat and shear than PVC, output only approx. half of PVC-U
|
|